The authors have recently observed a giant electrocaloric effect (12 K in 25 V) in 350 nm sol-gel PbZr(0.95)Ti(0.05)O(3) films near the ferroelectric Curie temperature of 242 degrees C. Here the authors demonstrate a giant electrocaloric effect (5 K in 25 V) in 260 nm sol-gel films of the relaxor ferroelectric 0.9 PbMg(1/3)Nb(2/3)O(3)-0.1 PbTiO(3) near the Curie temperature of 60 degrees C. This reduction in operating temperature widens the potential for applications in cooling systems. (c) 2006 American Institute of Physics. (DOI:10.1063/1.2405889)
Description
Keywords
Pyroelectric properties , Ceramics , Pb(mg1/3nb2/3)o-3-pbtio3 , Relaxor ferroelectrics , Lead , Ozone , Dielectric properties , Ferroelectric thin films
Citation
Mischenko, A. S., Zhang, Q., Whatmore, R. W., Scott, J. F. and Mathur, N. D. (2006) 'Giant electrocaloric effect in the thin film relaxor ferroelectric 0.9PbMg1∕3Nb2∕3O3–0.1PbTiO3 near room temperature', Applied Physics Letters, 89(24), pp. 242912. doi: 10.1063/1.2405889
Link to publisher’s version
Copyright
© 2006 American Institute of Physics.This article may be downloaded for personal use only. Any other use requires prior permission of the author and AIP Publishing. The following article appeared in Mischenko, A. S., Zhang, Q., Whatmore, R. W., Scott, J. F. and Mathur, N. D. (2006) 'Giant electrocaloric effect in the thin film relaxor ferroelectric 0.9PbMg1∕3Nb2∕3O3–0.1PbTiO3 near room temperature', Applied Physics Letters, 89(24), pp. 242912 and may be found at http://aip.scitation.org/doi/abs/10.1063/1.2405889