Interfacial modulus mapping of layered dental ceramics using nanoindentation
| dc.contributor.author | Theocharopoulos, Antonios L. | |
| dc.contributor.author | Bushby, Andrew J. | |
| dc.contributor.author | P'ng, Ken M. Y. | |
| dc.contributor.author | Wilson, Rory M. | |
| dc.contributor.author | Tanner, K. Elizabeth | |
| dc.contributor.author | Cattell, Michael J. | |
| dc.contributor.funder | State Scholarships Foundation | en |
| dc.date.accessioned | 2017-01-20T15:21:54Z | |
| dc.date.available | 2017-01-20T15:21:54Z | |
| dc.date.issued | 2016-12-15 | |
| dc.date.updated | 2017-01-20T15:14:12Z | |
| dc.description.abstract | PURPOSE: The aim of this study was to test the modulus of elasticity (E) across the interfaces of yttria stabilized zirconia (YTZP) / veneer multilayers using nanoindentation. MATERIALS AND METHODS: YTZP core material (KaVo-Everest, Germany) specimens were either coated with a liner (IPS e.max ZirLiner, Ivoclar-Vivadent) (Type-1) or left as-sintered (Type-2) and subsequently veneered with a pressable glass-ceramic (IPS e.max ZirPress, Ivoclar-Vivadent). A 5 µm (nominal tip diameter) spherical indenter was used with a UMIS CSIRO 2000 (ASI, Canberra, Australia) nanoindenter system to test E across the exposed and polished interfaces of both specimen types. The multiple point load – partial unload method was used for E determination. All materials used were characterized using Scanning Electron Microscopy (SEM) and X – ray powder diffraction (XRD). E mappings of the areas tested were produced from the nanoindentation data. RESULTS: A significantly (P<.05) lower E value between Type-1 and Type-2 specimens at a distance of 40 µm in the veneer material was associated with the liner. XRD and SEM characterization of the zirconia sample showed a fine grained bulk tetragonal phase. IPS e-max ZirPress and IPS e-max ZirLiner materials were characterized as amorphous. CONCLUSION: The liner between the YTZP core and the heat pressed veneer may act as a weak link in this dental multilayer due to its significantly (P<.05) lower E. The present study has shown nanoindentation using spherical indentation and the multiple point load - partial unload method to be reliable predictors of E and useful evaluation tools for layered dental ceramic interfaces. | en |
| dc.description.status | Peer reviewed | en |
| dc.description.version | Published Version | en |
| dc.format.mimetype | application/pdf | en |
| dc.identifier.citation | Theocharopoulos, A. L., Bushby, A. J., P'ng, K. M. Y., Wilson, R. M., Tanner, K. E. and Cattell, M. J. (2016) 'Interfacial modulus mapping of layered dental ceramics using nanoindentation', J Adv Prosthodont, 8(6), pp. 479-488. doi:10.4047/jap.2016.8.6.479 | en |
| dc.identifier.doi | 10.4047/jap.2016.8.6.479 | |
| dc.identifier.endpage | 488 | en |
| dc.identifier.issn | 2005-7806 | |
| dc.identifier.issued | 6 | en |
| dc.identifier.journaltitle | Journal Of Advanced Prosthodontics | en |
| dc.identifier.startpage | 479 | en |
| dc.identifier.uri | https://hdl.handle.net/10468/3491 | |
| dc.identifier.volume | 8 | en |
| dc.language.iso | en | en |
| dc.publisher | Korean Academy of Prosthodontics | en |
| dc.rights | © 2016 The Korean Academy of Prosthodontics. This is an Open Access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/by-nc/3.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited. | en |
| dc.rights.uri | https://creativecommons.org/licenses/by-nc/3.0/ | en |
| dc.subject | Elastic modulus | en |
| dc.subject | Fluorapatite | en |
| dc.subject | Zirconia | en |
| dc.subject | ~Cork University Dental School and Hospital - Journal Articles~ | en |
| dc.title | Interfacial modulus mapping of layered dental ceramics using nanoindentation | en |
| dc.type | Article (peer-reviewed) | en |